Publication:
Evaluation of Surface Roughness of Nanofilled Composite Restorations after Simulated Tooth Brushing using Various Dentifrices

creativeworkseries.issn1812-2027
dc.contributor.authorRana, M
dc.contributor.authorUpadhya, M
dc.contributor.authorJaiswal, A
dc.contributor.authorTyagi, K
dc.date.accessioned2025-11-23T08:08:11Z
dc.date.available2025-11-23T08:08:11Z
dc.date.issued2018
dc.descriptionRana M,1 Upadhya M,1 Jaiswal A,2 Tyagi K3 1Department of Conservative Dentistry and Endodontics 2Department of Orthodontics 3Department of Oral Pathology M.B. Kedia Dental College, Birgunj, Nepal
dc.description.abstractABSTRACT Background Teeth restored with direct composite resin are constantly exposed to specific challenges of the oral cavity. These challenges can modify the material properties and, when associated with daily brushing, eventually change its surface roughness, allowing bacterial growth and retention of extrinsic pigments. Dentifrices plays an important role in dental wear (abrasion) and over time, can also cause an increase in the surface roughness of restorative materials. Objective To assess the effect of dentifrices on the longevity of direct nanofilled composite resins restorations as far as wear and roughness is concerned. Method Class V cavity were prepared on 90 extracted human teeth and restored with Filtek Z350 composite. Teeth were randomly divided into 6 experimental groups of 15 each labelled as Group-1 (Colgate Dental cream) Group-2 (Colgate Active Salt toothpaste), Group-3 (Pepsodent Regular toothpaste), Group-4 (Dabur red toothpaste), Group-5 (Dabur Lal tooth powder) and Group-6 Control (water). The samples were fixed on tooth brushing machine and subjected to mechanical tooth brushing using various dentifrices according to respective groups in 3 phases and reading of surface roughness (Ra) was recorded. Result Surface roughness (Ra) had increased in following order: Group 6 < Group 3 < Group 2 < Group 1 < Group 4 < Group 5. All the tooth pastes were compared, their behaviour was found to be similar as there was no statistically significant difference amongst them. Though all of them were inferior to control group and the difference was statistically significant. Whereas the only tooth powder Dabur lal tooth powder gave the maximum roughness when compared with the other tooth pastes and the difference was statistically significant. Conclusion With increase in time of brushing there was increase in surface roughness in all the 5 dentifrices among them Ra was maximum for Dabur lal tooth powder. KEY WORDS Dentifrices, Filtek Z350 composite, Surface roughness (Ra)
dc.identifier.urihttps://hdl.handle.net/20.500.14572/3222
dc.language.isoen_US
dc.publisherKathmandu University
dc.subjectDentifrices
dc.subjectFiltek Z350 composite
dc.subjectSurface roughness (Ra)
dc.titleEvaluation of Surface Roughness of Nanofilled Composite Restorations after Simulated Tooth Brushing using Various Dentifrices
dc.typeArticle
dspace.entity.typePublication
local.article.typeOriginal Article
oaire.citation.endPage236
oaire.citation.startPage231
relation.isJournalIssueOfPublication9413a8eb-6c9b-4953-b728-96cdafea83bb
relation.isJournalIssueOfPublication.latestForDiscovery9413a8eb-6c9b-4953-b728-96cdafea83bb
relation.isJournalOfPublicationa782b7ff-cf89-4178-ad1c-11ed89cfe1bd

Files

Original bundle
Now showing 1 - 1 of 1
Loading...
Thumbnail Image
Name:
231-236.pdf
Size:
471.09 KB
Format:
Adobe Portable Document Format
License bundle
Now showing 1 - 1 of 1
No Thumbnail Available
Name:
license.txt
Size:
1.86 KB
Format:
Item-specific license agreed to upon submission
Description:

Collections